  1. moseley

    S41008 (410s) P7 PWHT Conditions?

    I have a project currently underway which involves .500" SA-240 Type 410s (P7 Gr. 1) and the client is imposing a MDMT/CET of -20°F. We have completed the production impact plates as required by ASME VIII-1 (UHA-51(h)) and according to UHA-32 the PWHT of this material is required to be performed...
  2. moseley

    304ss Coating

    Can anyone enlighten me on the use and reason of coating A312 TP 304L piping in LNG service. This piping will be in a Cryogenic service and will also be insulated. Thanks for any information.
  3. moseley

    Welding Calculation

    Can anyone lead me to a calculation to find inches of weld in different groove designs? I have searched the internet and numerous Engineering sites for the formula with no help. Thanks in advance for some help!
  4. moseley

    Hartford Boiler Handbook

    Can anyone lead me to the site to order a Hartford Boiler Handbook? I understand that this book has more information than the pipefitter bluebook (just for basic info). Thanks in advance for any help
  5. moseley

    Brinell Hardness Values

    Can anyone point me to the literature which gives brinell hardness acceptable ranges for materials. Thanks in advance for any help.
  6. moseley

    Recommended Installation

    Could anyone help, I have a question regarding the installation of Screwed and Socket-welded Unions. I have ran across some unions installed wrong. I can't find anything documenting that the nut should be on the flow side, I know this is probably "rule of thumb". Can anyone point me in...
  7. moseley

    Blushing on Urethane

    Has anyone ever encountered any blushing problems on a Epoxy/High Gloss Urethane paint system. We completed a job about a year ago,and 4 months after completion the lines started to show considerable blushing (blotches) through out the project. The lines operate from ambient to occassional 120...