I want to increase the hardness of 17-4 H1100 from 36 Rc to 45 Rc;
Do a supplementary heat treatment at 900F (H900) is enough or do I need to do a solution heat treating before?
Hi,
I need a little help for welding heat resistant stainless steel casting alloys (similar to ASTM A 351 gr HT)
Is anybody having some information to share about: what welding rod better to use, pre-heat temps, cooling speed, and post-weld heat treatment if any...
Thank you