  1. Turda

    cryogenic process

    I anybody using deep freezing(-300F) as a part of the process. Is it realy worth the money? Thank you, Turda
  2. Turda

    cryogenic process

    I anybody using deep freezing(-300F) as a part of the process. Is it realy worth the money? Thank you, Turda
  3. Turda

    welding SS310

    Hi, I need to calm down a staborn customer which insist in welding repairs for his SS310 carburize fixtures. I now from experience that once carburized, the welds wont last more than few runds.I need few direction to start make a presentation based on theory. What book or resources should I use...
  4. Turda

    8620 surface perlite

    Hi, I realy have hard time dealing with surface perlite for carburized 8620. I'm using endo and the case depth I'm aiming for is .030". I'm looking for any tips to reduce surface perlite/bainite. Thank you, T
  5. Turda

    9310 carb

    Hi, I realy have hard time to obtain a surface hardness of 60-61 HRC on 9310 carburised steel.Finaly I've found a way to get less retained austenite (>15%) but surprise.....58 HRC only. Any ideas way? 9310 FUN