I need to compare H1150 vs H900 in an axially loaded part. The H1150 parts have failed where expected(stress conc.) and I wonder if H900 will fill the bill even though the Ut of H900 indicates severe brittleness. For reference, the machined surface finish is 32 Ra and the stress concentration...