  1. Olcay

    Stress Corrosion Test

    Situation: We are heat treating a part made of sheet metal 50CrV4 used as clamp. There is a test for stress corrosion as : Put the parts under stress, in a 0,9% HCl solution, and they must stand at least 8 minutes before broken. Problem: We could not solve which parameters of hardening and...
  2. Olcay

    Stress Corrosion Test

    Situation: We are heat treating a part made of sheet metal 50CrV4 used as clamp. There is a test for stress corrosion as : Put the parts under stress, in a 0,9% HCl solution, and they must stand at least 8 minutes before broken. Problem: We could not solve which parameters of hardening and...