Can an one help me determine a possible material for this application. I acts as a brake type pad and is made up of the following material.
Molybdenum : 43%
Niobium: 18%
Tungsten: 30%
Iron: REM
why would you use Niobium?
Thanks,
Below is a material analysis results and hope someone can help out.
C .30%
Mn .36%
P <.010
S <.001
Si .30%
Cr 12.03%
Ni .08%
Mo .27%
Cu .02%
Al <.01
Sn <.01%
Hardness 34 HRc