  1. snydes5048

    Fabricating a frustrum of a cone

    Need to make a frustrum of a cone using niobium-30w/oTi-20w/o W alloy. 0.5-inch wall thickness. Two possible fabrication techniques have been posed. Use powder met and HIP to near net shape. Roll plate and form and seam weld. The later isn't attractive for several reasons. Does anyone know...