    Delaying PWHT of a Pressure Vessel after Completion of Welding

    Is it inadvisable (or bad practice) to delay PWHT of a 1.25Cr0.5Mo Pressure Vessel with a wall thickness of up to 133mm (Hydrogen Service)? Low hydrogen consumables have been used. Appropriate Pre-Heats and post heating / DHT have been applied. Why is this even a concern? Logically, since on...
  2. deics

    Dark Patches on Bores of SS321 Tubes

    Problem - After a tube leaked in a new exchanger under a hydro test all tubes were checked with ECT and some were found to give indications above reference level. Tubes were checked by fiberscope. Spiral marks resembling roll straightener marks were seen in the bores. The tube that leaked had...