    Fired Heater tube corrosion

    A Fired Heater with a hydrocarbon process gas containing 1 mol% H2S and tubes of ASTM 106 Gr B suffered rapid internal corrosion at the tube outlets ie 4mm in 1.5 years. Process gas outlet conditions are 295 degC at 65 barg and the gas is dry. The scale is a mixture of iron oxides and sulfides...
  2. DonT

    Fired Heater tube corrosion

    A Fired Heater with a hydrocarbon process gas containing 1 mol% H2S and tubes of ASTM 106 Gr B suffered rapid internal corrosion at the tube outlets ie 4mm in 1.5 years. Process gas outlet conditions are 295 degC at 65 barg and the gas is dry. The scale is a mixture of iron oxides and sulfides...