  1. azer mashhood

    PWHT on corrosion resistant alloy piping

    Hi, Appreciate if somebody can provide some guidance here. We have a carbon steel base pipe (more than 20mm thick) with Alloy 626 clad. Sour service at fairly high pressure offshore application. Does the base metal require PWHT? If the base metal hardness is maintained with pre heating and...