I'm working on some tolerances after cool down, and have up until now been using CTE's; typically 17,3um/mK for 304SS, 16um/mK for 316SS, and 16,7um/mK fro BeCu
I've been refining my design, and have been double checking with the NIST cryo materials page, where I have worked out expected...