  1. nihil88

    degassing process of white cast iron

    hello there, i have problems. when we poured high chr. white cast iron in molds, metal melt has boiled in sprue. we tried degassing technique with Al turnings, but more didnt not work. a lot of gas porosity,and shrinkage too. we cast high. white cast iron aprrox. 1500 celcius degree and...
  2. nihil88

    high chromium white cast iron nucleation

    I m a material engineer and work in a foundry. we produce high chromium white cast iron abrasive balls. we cannot use %100 returns in smelting due to inhibition of starting nucleation. But we use pig iron for starting nucleation grey-ductile iron smelting. i want to produce high chr white...