Hi everybody!
Need an advise on steel heat treatment please. A drawing specifies induction hardening 56-61 HRC with 3mm case depth for a 42CrMo4 steel pin 200mm in diameter. The supplier claims that in this case only hardness 50-55 HRC is achievable. The engineer that made the drawing refers to...