  1. AndreLuizPaiva

    Abnormal grain growth during annealing (decarburization layer)

    Hello everybody, I've been experiencing a problem with continuous furnace for annealing. The working cycle takes about 1,5h to reach its peak (750ºC (1-2 hours)), then decreases to 720ºC (5 hours). In a particular sample, a SAE 1010 welded tube (6,3 mm thick, outer diameter 63,5 mm) , there is...