Here's the situation. We cold form our heads for pressure vessels using 9% Ni plate (A553 and A353, mostly A553 though), and stress relieve the heads after forming. We closed a plant in Plaistow, NJ and inherited (paided for) a bunch of heads from that facility. Problem was, they didn't have...