Oops, I was unclear. I have a production manager who insists that 440C will undergo PERMANENT shrinkage when heat treated (specifically to Rockwell 58-62C)
The only reason I can think of is that the martensite is changing to ferrite and cementite, which is causing an EXTREMELY small amount...