Thanks a bunch for your imput. I myself have designed them
and have used 4140 hardened to Rc 38-42. I have always
seemed to have good luck, but the last ones I designed
are failing. I am researching how our shop processed
them, I am suspicious that they have done something to
cause this. Once...