Are there standards for a minimum or/and maximum turns of teflon tape on a give NPT thread. In my company we use 1.5 to 2 turns, but not sure.
TIA,
Alfonso Del Toro
metengr:
Thanks a lot for your inputs. Unfortunately, we cannot use teflon tape since this nut handles are designed for multiple engagements. I will contact our supplier about electroless plating and see if that is a viable route. Again, thanks a lot for your help.
Hello all,
We have a number of brass (half hard)nuts that have been nickel plated that do not meet specs. We can re-tap them to meet those dimensions, but during that process the nickel platting will be removed. Does anybody have any data, or a reference, as to what the wear rate would be for...
Hello,
We are having solder flow problems on a nickel plated battery terminal. Using flux is not helping until the terminal is heated a lot. This takes a lot of time, with not very nice solder results. Any ideas on how to pre-clean will be appreciated.
Thanks,
Alfonso Del Toro