the thickness of these plates are 1" and 1.5". They have not specified the depth of the single groove. The fabricator claims to have done this for other companies in the past, supposedly they know what they are doing. My concern is that in theory, this may work - welding two plates together...
Yes, L10x10. They are proposing to do a butt joint single V groove weld between two plates. I'm sorry, I am new to this forum... what is PJP or CJP? Yes, the slower alternative is importing the section from India.
Hello,