First thank you for the quick resonds.
The 410S is no longer going through the pressure boundry (due to failing to pass impact testing) we have changed the design (repaced a rolled 410S plate that maked a 16" nozzle with a 16" SA 106-B pipe and weld overlay). There is a 410S 6" internal...
First thank you for the quick resonds.
The 410S is no longer going through the pressure boundry (due to failing to pass impact testing) we have changed the design (repaced a rolled 410S plate that maked a 16" nozzle with a 16" SA 106-B pipe and weld overlay). There is a 410S 6" internal...
I’m looking for some advise on welding 516-70 carbon steel to 410S stainless. I made some new PQR’s using 5/16 and 3/16 plate with .035-309L – HiSil hardwire, with our Lincoln STT for a open root. Then proceeded to cap it with 309L flux core. The bend test failed on the face side (It split on...
I’m looking for some advise on welding 516-70 carbon steel to 410S stainless. I made some new PQR’s using 5/16 and 3/16 plate with .035-309L – HiSil hardwire, with our Lincoln STT for a open root. Then proceeded to cap it with 309L flux core. The bend test failed on the face side (It split on...