    Need help with ideas on best for coating

    @3DDave, yes I want to coat the inside diameter. The coating itself can be superficial as the material readily bonds to the coating. I was experimenting just having a bucket of liquid coating and just dunking the tubing all together. At the end of it, it's no more than .1 mm coating given that...
  2. Shoura

    Need help with ideas on best for coating

    Thanks @IRstuff viscosity is about 0.013 Pa s. The coating adheres to the tube material. I'll look into spin coating. Thanks for the suggestion
  3. Shoura

    Need help with ideas on best for coating

    Hello, I and working to design a pilot assembly line where I am trying to coat a hollow tube. The coating liquid used needs to be heated to about 60+ degrees centigrade. The main issue is that the liquid will become solid at room temperatures and will create an unnecessary amount of the coat...