Recent content by RyanWengTW

  1. RyanWengTW

    AISI 4130 heat treatment

    oh! So the whole procedure will be: normalization > rough machining> water quenching and tempering > normalization ? Just want to make sure I'm not misunderstanding your suggestion.
  2. RyanWengTW

    AISI 4130 heat treatment

    Yeah, I've read metengr's recommendation. I'll let my boss and the consultant know maybe we have a better way to deal with it. Really appreciate!
  3. RyanWengTW

    AISI 4130 heat treatment

    The wall thickness would be 35mm. Thank you for the mention.[glasses]