    Black Corrosion Product on Electroless NiP in PBS

    Currently there is no heat treatment. I was under the impression the heat treatment would worsen the corrosion affect due to amorphous -> crystalline transition and formation of grain boundaries to attack. The substrate is cobalt-chrome, not because it is what will be on the final product, but...
  2. RJKing

    Black Corrosion Product on Electroless NiP in PBS

    Hello, Electroless Ni-P is a new product for me, but I have been assigned some research regarding the process. One of the qualitative preliminary tests I am running is to submerge samples in saline solution to analyze potential corrosion behavior. What I have noticed is that after about 2...