Hello,
We recently tested a pipe weld in As-Welded and PWHT condition for Weld Procedure Qual.
The Charpy results from Weld shows 5, 7 and 170 ft-lbs, the HAZ (Center of HAZ) shows 7, 60, 138.... I made sure that the samples were
extracted from the Weld and HAZ. One of the broken HAZ...