Thank you Qalander,
FYI, the LVGO rundown temp is 50-70C. We have managed to inject antioxidant from several company product but it's still not show any improvement.As you mentioned of material presence in LVGO, what is the most critical of material concern in this stream. One of our vendor...
Dear all,
Our LVGO became darker after a week rundown to storage tank. What is the solution to avoid discoloration problem? FYI, we use LVGO to blend into AGO instead of HVGO.
Thanks.
All,
What should I do for my storage tank (external floating roof type, which Working Press. is atm) if I will store hot naphtha(max. 50degC) at least 10 days without product cooler? Is the increment of RVP of hot naphtha will affect the tank?