Recent content by ld25

  1. ld25

    High purity water corrosion of Stainless

    Does molybdate or nitrate have any corosion protection of stainless in a cooling water loop? If so, is one better than the other? Does anyone know of any good links for the corrosion protection of stainless?
  2. ld25

    MIC prevention in stainless

    I have a cooling water loop that feeds a high temp furnace. 95% of the system is 316/304 SS including the furnace. What type of chemicals should I add to prevent MIC on the welds. The chlorides are about 2-7 ppm. Also, does Sodium Molybdate have any corrosion benifite for stainless cooling water...
  3. ld25

    Cooling Water Treatment

    I currently am expiriencing weld failures on a cooling water jacket on a high temp stainless furnace. The situation is as follow: System 95% 316L and 304 stainless 5% copper and bronze ~7ppm chloride levels Is there any type of chemical to help protect the welds from pitting and failure...
  4. ld25

    High iron content in chilled water loop

    Is there a type of chemical treatment that can be put into a chilled water loop that will keep iron particulate <.5um in solution even if it passes through a magnet coil? Thanks