  1. LBlount

    Possible galling between 18.8 S/S and 303 S/S

    Change the surface characteristics see thread: thread307-69863 [medal]
  2. LBlount

    How to stop hydrogen permeation during gold plating of a SS diaphragm?

    I concur with Jim. Instead of chemical plating try thin film coating. No Hydrogen present! Evap will keep temps below 125 degrees. Use plasma to sputter the surface and vacuum will extract most of the excess gasses if you leave it in long enough. Quite a set up for one project.
  3. LBlount

    Stainless Steel and Anti-Galling Lubricants

    Steve, I posted a solution for galling in another thread. thread338-52413 Galling on stainless steel thread under seawater condition. Try there! LeGrande