thanks for the link. My dies are about 8" across the face.
10" tall and mostly flat. with a few rings on them. I make net forgings. That pic is it ceramic costed or is the ceramic in the subtrate?
Thanks for the reply again. I called this guy Refmet. while the technology sounds interesting I don't get the impression that they are professional. I will log on at 7:30AM on May 5th 2006 leave me a link please and thank you.
yes I would be interested in having someone look at my process. I do warm forging with a 1500 ton mechanical press.
I forge 1100 degree c, 44mm, 1000 gram,.35 carbon steel.
I use a 100% soluble sodium hydroxide base lubricant.
I had heard of a company called Refmet that say they can diffuse the...
I'm intereted in using the ceramic diffusion process in my warm forging net shape forging I use H13 and I'd like to know who i could contact so as to try improving my die life and lubricity through this process. Anyone know who I could contact on more info?