I am working with 6061-T6 Aluminum seamless tube and 303 Stainless for the journals.
I looked in the Machinery's Handbook, but didn't see any info. on the Coefficient of Expansion for Aluminum. There was info for other materials, but not Aluminum. Do you have any specifics to find it.
I am looking for formulas and advice for heating an aliminum tube to allow S.S. journals to be inserted producing a shrink fit. I want to calculate the proper sizing if each item as well as the temp. needed for this operation to work properly.
Any help would be greatly appreciated.
Thanks JonWade
I am looking to find dimensional and cross referencing info on the following drawing note: "center hole should be according to JIS B 0041-A1. b/3.35"
Any help would be appreciated.