G275SP-1 is a Pearlitic Matrix Grey Iron with Minimum Tensile Strength of 275MPa. Hardness Range is 187 - 285 HB.
Typical Composition:
C 3.15 - 3.55
Si 2.15 - 2.55
Mn 0.50 - 0.60
Cu 0.25 max
S 0.16 max
P 0.10 max
Cr 0.25 max
Mo 0.40 - 0.60...
GM274M is a standard which covers a range of grades, firstly general purpose grades where Minimum Tensile can range from 125MPa to 250MPa. Followed by special purpose grades for Disc Rotors, Pump Bodies, Bearing Caps, Piston Rings and Cylinder Liners.
For the general pupose grades, the...
Can you please tell me, which is the better configuration for Pro-E.
4 drives - as 2 drives C: & D: mirrored.
4 drives - 1 large drive RAID 0/1 (striped & mirrored).
2 drives - 2 drives.
Does anyone have experience in flame hardening localised areas of coreboxes made of grey iron,used in the making of shell cores to extend the wear life? I am looking at alternative methods of extending our tool life.
I am looking for alternative materials to use for patterns in our high pressure sand moulding foundry. We are currently using P20 Tool Steel, sometimes nitrided. With certain pattern geometries, the patterns will wear beyond the accepted dimensional tolerance before expected. What materials do...