The standard A860 is more strict in both chemical and mechanical requirements, you can use WPHY 42, 46 and maybe WPHY 52 as WPL6 , when the tensile strength is not over 95 ksi, the yield strength,elongation and charpy values are lower for WPL6 with not maximum values. The WPL3, WPL8 and WPL9 are...