HELLO EVERYONE, I HAVE A TRICKY PART FOR TOOLING.
IT IS A DIAPHRAGM COMPONENT WITH A W/T OF 0.25mm.
ITS APPROX DIMENSIONS ARE 20mm SQUARE WITH A 2mm
HOLE THRO THE TOP FACE. THE SIDE AND TOP FACE ARE
A 3D FORM (MUCH LIKE A TEAT ON A BABIES BOTTLE BUT
IT HAS NO UNDERCUT). MY PROBLEM IS THAT THE...
I am thinking of moulding a PVC part, the grade is t.b.a.
I was wondering if anyone had any mould experience with PVC.
I was thinking of using pre-toughened stainless steel 1.2316
for the core & cavity plates as these appear to be good for a textured finish, as well as being resistant to the...
I have been given the job of quoting for new moulds.
Not very experienced in this and wondered if anyone can give me any advice/software that can help me in my quest for new work?
I have a tool to quote. It is basically a 22mm o/d tube , 6mm long with a flange to eject on at the bottom. It has a 1mm w/t. The problem I have is that it has a 0.4mm deep undercut ring all around the i/d. It is to be made from PEI - Ultem 1000. I dont have much experience with this and was...
the tolerance is in mm,
the steel part will be overmoulded in nylon,
no flash allowed
the whole steel part is covered in plastic (top, bot & sides) except for some pads on the top & bot face of the steel part which need to s/o in the tool.
There is a hole up the centre of the part which is...
I have to design an injection mould which moulds over a steel part. This is no problem except for the tolerance of the steel part. It is +.5, -.5. Any ideas how to soak up the tolerance in the tool?