T joint is the configuration. At first sight, I have choice between a 309 grade or a CS filler metal but, would these material could cause chemistry problems ? Should I weld annealed ? Before or after H1050 conditionning ?
I have to do a fillet weldment between a 2" thickness 17-4ph H1025 plate and a 1 1/2" A36 or 44W plate. Weldment profile is 5/16" wide. I have to elaborate procedure and I'm looking for the better filler metal.
Should I weld on annealed plate and is it safe to make heat treatment...