    Deposits in pipes

    Coming from a mineral processing background, we generally have a rough rule of thumb of over 2 m/s line velocity for settling slurries. If there is a lot of coarse and/or low density (ie less hindered settling) and we know there will be a problem with sanding, then 4-5 m/s is typical. There is...