We have a process where we run pulse welds of ~40 Mil diameter spots across a Cobalt to mild steel(hardened) seam interface. At one point we had good, clean, smooth welds, but recently we are getting a large generation of soot, carbon, spitting, pitting, and slag on/around our weld interface...