I need to run a Weibul Analysis for my testing and am looking for some information about it. I have never used it before for testing and not exactly sure what it is. I have to meet a R95C90 level form my tests. I've looked at some brief Weibul examples on the web but am still a little...
I mean extruding the steel end fitting (reducing its size) in a solid die onto the wire. The end fittings are loaded in a cartridge on the extruding die. You insert the wire into the extruder that has a end fitting in place and it exturdes the piece on. I hope this clears it up.
I am currently extruding a steel end fitting on to a wire for my assembly. The steel end fitting is currently coated with a phosphate & wax for corrosion resisitance. The phosphate & wax coating does not meet the corrosion requirments, so I need to look for an alternative. However, in the...
I can not have a secondary process to coat these parts after they are extruded due to the fact that this in done on the assembly line when the complete assembly is built. What type of plating could withstand the extruding process without scraping off or damaging the dies? The Phosphate plating...
I am investigating corrosion protection on an extruded component. We have steel end fittings that are extruded onto wire. This component is under the vehicle and must meet SAE J2334 test requirements as follows
1 year Appearance Requirement – 15 Cycles SAE J2334 – Immersion Method (1 rating...