  1. Billy Le

    Mechanical Failure - High Yield

    Good morning, I am new to the heat treating process. We got the 7050-T74 aluminum test results - Failed yield. S/B 72.0 ksi max. measured at 73.6 ksi. Please advise if we can rework? and how to rework. In addition, is there any website (links) to learn how to rework and which process to rework...