Hi Ron , thanks for your answer.
The concrete for those two floors were of 25 mpa.During the curing period the concrete was kept soaked for two weeks with a plastic on top and was monitered constantly through out this time.The stone size was 3/4 inches.We used super plastifier to keep the water...
Subject: curling problems in our buildings
Hi,we are having curling problems in two of our buildings.One of the building is a refrigarator,the other one is a printing facility.
We have novocon steel fiber in both floors 30 pounds per cubic meter ,six inches slab,lazer screed,water cured for...