    E-coat problems

    Thanks for the help TVP and gdodd. I've tried to mark it down as helpful but the system will not let me! I will keep trying. thanks Neil
  2. 210269

    E-coat problems

    What can cause e-coat problems. Bubbling can be found in certain areas on the vehicle,(is this caused by the e-coat being to hot,oil or Chemical reaction with sealant)Rust is comming through where bubbling and sealant is found. please help!
  3. 210269

    plastics

    Is there a cost effective plastic /acrylic in manufacture that when used as clear glazing or partition in a vehicle that can meet all EU testing, ie abration strength ect.I Know of a material called Lexan from an American company but this is very costly.
  4. 210269

    welding of neotec material

    dKelly, Thanks for your help
  5. 210269

    welding of neotec material

    There is a new material my company want to use for our fuel tank which is called neotec (supplied from curos. The problem i have is the spot welding and seam welding is poor do you have any ideas of improving this.