INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Composite coating for SS to be buried underground

Composite coating for SS to be buried underground

Composite coating for SS to be buried underground

(OP)
What would be a good way to composite coat SS piping to efectively make it more corrossive reistance and waht are the right materials for this application. We intend to use 316 ss piping and have some concernse about corrosion if buried by itself witout protection. Any sugestios welcomed.

RE: Composite coating for SS to be buried underground

Without knowing exactly what you are doing, there are heat shrink/hot melt products that are available. Basically you slide the heat shrink tube over the part and warm it up with a hot air gun. The sleeve shrinks and inside the sleeve is hot melt glue which melts at the same time and totally encapsulates the part; usually this system is to permanently protect high voltage buried electric cable.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.