HELP WITH BOLTS ASTM - A-563 GR. A OR B
HELP WITH BOLTS ASTM - A-563 GR. A OR B
(OP)
Greetings from Peru.
Hi, my name is John Altamirano; I am Mechanical Engineer.
I have a problem and it's about Bolts.
I need some help.
I have to buy Hexagonal Bolts ASTM A-563 Grade A (5/8", 3/4", 1") and Grade B (1/2").
After looking at the local market. I found there aren't Bolts with those features.
I would like to know if there are equivalents to those bolts for buying them instead the first ones
because I just need few pieces of these. And I am not thinking to buy them abroad.
I thanks anyone who can help to solve my problem.
And I will appreciate if you can answer my question as soon as it can be.
John Altamirano A.
Dpto. Compras
FIMA S.A. - PERÚ
(051-1) 452-2212 (270)
www.fimaperu.com
Hi, my name is John Altamirano; I am Mechanical Engineer.
I have a problem and it's about Bolts.
I need some help.
I have to buy Hexagonal Bolts ASTM A-563 Grade A (5/8", 3/4", 1") and Grade B (1/2").
After looking at the local market. I found there aren't Bolts with those features.
I would like to know if there are equivalents to those bolts for buying them instead the first ones
because I just need few pieces of these. And I am not thinking to buy them abroad.
I thanks anyone who can help to solve my problem.
And I will appreciate if you can answer my question as soon as it can be.
John Altamirano A.
Dpto. Compras
FIMA S.A. - PERÚ
(051-1) 452-2212 (270)
www.fimaperu.com





RE: HELP WITH BOLTS ASTM - A-563 GR. A OR B
Use A 325 or A 449 for structural bolts.
RE: HELP WITH BOLTS ASTM - A-563 GR. A OR B
The bolts should be:
ASTM A 325 or A 490
Both should be bought as a set bolt and nut.