INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Alloy 24 Cr Ni Mo 554V

Alloy 24 Cr Ni Mo 554V

Alloy 24 Cr Ni Mo 554V

(OP)
Can someone please assist in providing the chemical analysis and mechanical properties for 24 Cr Ni Mo 554 V ?
And an  equivalent North American alloy would be great.
Thanks to all in advance.
mac

RE: Alloy 24 Cr Ni Mo 554V

Double check the grade, there is a 24NiCrMoV14-6, and a bunch with similar designations.  Do you have a specification No. or an alloy No.?

= = = = = = = = = = = = = = = = = = = =
Corrosion never sleeps, but it can be managed.
http://www.trenttube.com/Trent/tech_form.htm

RE: Alloy 24 Cr Ni Mo 554V

(OP)
Sorry, can't provide more info.  I suspect that this is a "house designation" to keep the client coming back to the O.E.M..  However, I now am advised that this component has been previously supplied in 4340 H.T.S.R. and that is an apparently satisfactory alternate.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources