17-4PH 17-7PH Tubing
17-4PH 17-7PH Tubing
(OP)
Guys,
I am in need of 17-4PH per AMS 5643 or 17-7PH per AMS 5568 tubing. They should be approx. 44 inch in length, .749 OD and .590 ID.
Do you know any manufacturer that can help me with this? The vendor we have gives us a lead time of 20 weeks and management is having a heart attack.
Thanks
I am in need of 17-4PH per AMS 5643 or 17-7PH per AMS 5568 tubing. They should be approx. 44 inch in length, .749 OD and .590 ID.
Do you know any manufacturer that can help me with this? The vendor we have gives us a lead time of 20 weeks and management is having a heart attack.
Thanks





RE: 17-4PH 17-7PH Tubing
RE: 17-4PH 17-7PH Tubing
= = = = = = = = = = = = = = = = = = = =
Corrosion never sleeps, but it can be managed.
http://www.trenttube.com/Trent/tech_form.htm
RE: 17-4PH 17-7PH Tubing
I checked with 2 suppliers, nothing at either one
What is the quanity needed of each material?
Here is one source that has been good in the past.
http://www.eagletube.com
RE: 17-4PH 17-7PH Tubing