INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

explain phenomena occurring before tube leakage

explain phenomena occurring before tube leakage

explain phenomena occurring before tube leakage

(OP)
I observed in our 500MW boilers prior to tube leakage,ammonia level in feed water and sat. steam is raising by 0.2ppm i.e from 0.45 (normal) to around 0.55 to 0.65 ppm. Explain how is this possible.

RE: explain phenomena occurring before tube leakage

It is most probably that the increased ammonia level caused the tube failures and not otherwise. I have observed this phenomenon in low pressure steam line in a ammonia plant - though I am not sure about the exact mechanism that causes this failure.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources