Photographs of Pipe Bursts Due to Waterhammer
Photographs of Pipe Bursts Due to Waterhammer
(OP)
I am preparing a paer on waterhammer. I would like to get hold of some photographs of pipe bursts that have resulted from waterhammer events. COuld anyone suggest a website or email me on blenrayaust@yahoo.co.uk
Many Thanks
Many Thanks





RE: Photographs of Pipe Bursts Due to Waterhammer
http://www.fisstate.org/mainline.htm#PART%202%20-%20Diagnostic%20Photographs%20&%20Examples
good luck
RE: Photographs of Pipe Bursts Due to Waterhammer
The biggest pipe burst event due to water hammer was in our memory the FOSTAD water pumping system in Egypt where around 1975 a DN 600 swing check behind a KSB pump bursted up the pipe like a sausage.
I have contacted KSB, but nobody had some photos on file.
- By the way, the problem was solved with a nozzle type non-slam check valve sold by Mannesmann Demag nowadays available at Noreva.
RE: Photographs of Pipe Bursts Due to Waterhammer
I have no photos I can tie directly to an "event", which I take to mean some specific component failure or horrible design flaw.
But I do have photos of pipe bursts due to what I would call pressure transients or surges that I linked directly to poor hydraulic design. All are PVC bursts.
I am not sure what your paper is going to be used for. I am willing to let you download the images if your paper is not going to be published formally, just shared within your company or amongst collegues. I need these photos myself for future publishing. The link someone gave above has my photos in it.
PUMPDESIGNER
RE: Photographs of Pipe Bursts Due to Waterhammer
RE: Photographs of Pipe Bursts Due to Waterhammer
There in lies the problem. No one wants their failures aired in public. It would appear that the insurance companies have bound up the evidence.