What is Chrome Steel (303)?
What is Chrome Steel (303)?
(OP)
I am looking at buying some knife gate valves for a slurry application. One of the two options available has a spindle made of stainless steel 304 and the other has a spindle made of chrome steel (303). What is chrome steel?





RE: What is Chrome Steel (303)?
http://www.matweb.com/search/SpecificMaterial.asp?bassnum=Q303A
Regards,
Cory
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.