(OP)
Can anyone tell me what the ASTM equivalent is to CuSn5Zn5Pb Brass? Also, where can I find a chart that shows all of the other equivalents?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Material Equivalents
ASTM B30 ;
ASTM B584 ;
ASTM B763 .
The corresponding UNS numbers may be UNS C83600 and/or UNS C83800.
Hope this helps,
'NGL
RE: Material Equivalents
Can someone tell me whether ASTM B-16 can be used for UV stamped safety valve or not?
I know it is prohibit to use the material unlisted in ASME Code Section ?, but I found many safety valve manufactured with brass, Can someone tell me whats the material used for?
I am designing a safety valve for apply for UV Stamp, can someone share me some experience? Thanks!