INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

About QW-404.5

About QW-404.5

About QW-404.5

(OP)
According to QW-404.5 a change from one A No. to any A No. needs requalification. but I cant understand the mean of this sentence:
 "qualification with A No. 1 shall qualify for A No. 2 and vice versa"
Could you explain this sentence?

Thanks
H.Mirhosseini

Regards
H.Mirhosseini

RE: About QW-404.5

In QW 404.5, a change in A - number requires re-qualification of a welding procedure with the exception of A-No. 1 and A-No. 2 filler metal compositions. Because of the similarity between the two A number filler metal compositions, you can take credit for both A-No.1 AND A-No.2 as long as one of the two filler metals has been deposited and qualified in the welding procedure.

RE: About QW-404.5

When I teach exam prep classes for API-653 and API-510 Inspectors I suggest that they write "A1=A2" in the margin of the Code as any easy way to remember this Code exception.

Steve Braune
Tank Industry Consultants
www.tankindustry.com

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.