What SMAW rod for 316SS to A36 structural?
What SMAW rod for 316SS to A36 structural?
(OP)
Guys what filler would you recommend for welding 316 to A36. This is a horizontal position weld to be made in the field. The part in question is a 316 beam bracket for a new pipe hanger, Power Piping Fig. 200, that I am fillet-welding to an existing A36 W10x_. Should I use a SS rod or can we use something like 5P-Plus?
Thanks for your help!
Thanks for your help!
Thanks!
Pete





RE: What SMAW rod for 316SS to A36 structural?
RE: What SMAW rod for 316SS to A36 structural?
RE: What SMAW rod for 316SS to A36 structural?
RE: What SMAW rod for 316SS to A36 structural?
Thanks!