INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Winch drum & flanges thickness

Winch drum & flanges thickness

Winch drum & flanges thickness

(OP)
How do i calculate the thickness of the drum & flanges
on a winch drum ?

Lenght 1,5m , D=1,2m , wiredia=32mm , flangedia=1,8m
linepull=48MT= 480000N

I tried to apply the DNV rules but got a 14cm wallthickness
on the drum.. overkill or not ?

brgds odd from norway

RE: Winch drum & flanges thickness

If you can get access to the "Design of Weldments by Omer Blodgett" the is method for the design of a cable drum in the “Steel Rolls Chapter”.   The example consolidates all the references from Timoshenko and Roark

The book can usually be purchased from any bookstore or directly from the website or it’s representative in Europe.

https://ssl.lincolnelectric.com/lincoln/spmount/item.asp?prodnum=DW

RE: Winch drum & flanges thickness

(OP)
Thanks a lot guys. Down to approx 3mm now,hehe
only size of flanges missing now
brgds

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources